first_layer_adhesion
Differences
This shows you the differences between two versions of the page.
| Both sides previous revisionPrevious revisionNext revision | Previous revision | ||
| first_layer_adhesion [2026/08/03 23:53] – dshoop | first_layer_adhesion [2026/08/03 23:55] (current) – dshoop | ||
|---|---|---|---|
| Line 38: | Line 38: | ||
| ==== First layer speeds too fast ==== | ==== First layer speeds too fast ==== | ||
| - | Try slowing down to 30mm/ | + | Try slowing down to 20-30mm/ |
| First layer speeds depend on filament material and other factors. Speeds for first layers tend to be under 60mm/s and as slow as 20mm/s for some filaments. | First layer speeds depend on filament material and other factors. Speeds for first layers tend to be under 60mm/s and as slow as 20mm/s for some filaments. | ||
| Line 56: | Line 56: | ||
| No. Glue on a PEI bed plate is used to form a separation layer to prevent printed parts from binding to the bed plate. | No. Glue on a PEI bed plate is used to form a separation layer to prevent printed parts from binding to the bed plate. | ||
| - | Glue was used on older types of printers that had glass or other material beds than textured PEI which grabs far sticker than glue. | + | Glue was used on older types of printers that had glass or other material beds than textured PEI which grabs far sticker |
| If glue is " | If glue is " | ||
/app/data/attic/first_layer_adhesion.1785815633.txt.gz · Last modified: by dshoop